[labnetwork] Question about Ocean Optics Nanocalc-DUV
Aebersold,Julia W.
julia.aebersold at louisville.edu
Wed Oct 20 10:42:52 EDT 2021
Filmetrics also sells standards that you can use to calibrate your instrument.
Cheers!
Julia Aebersold, Ph.D.
Manager, Micro/Nano Technology Center
University of Louisville
Shumaker Research Building, Room 233
2210 South Brook Street
Louisville, KY 40292
(502) 852-1572
http://louisville.edu/micronano/
From: labnetwork [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Shimon Eliav
Sent: Wednesday, October 20, 2021 5:09 AM
To: Malhotra, Sandra Guy <sandra.malhotra at tamu.edu>
Cc: Fab Network <labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Question about Ocean Optics Nanocalc-DUV
CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.
Hi Sandra,
We have the same equipment here at Hebrew University. It came without any reference, but we have a piece of Si with a known thickness of SiO2 and this serve us as reference prior any measurement. Very simple and useful.
Regards,
Shimon
The Hebrew University of Jerusalem
The Unit for Nano Fabrication
ISRAEL
From: labnetwork [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Malhotra, Sandra Guy
Sent: Tuesday, 19 October 2021 23:50
To: Fab Network <labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>>
Subject: [labnetwork] Question about Ocean Optics Nanocalc-DUV
Howdy All,
We recently encountered a situation where the halogen bulb in our Ocean Optics Nanocalc-DUV spectrometer stopped functioning and only the deuterium bulb was working, but this was not apparent, so we continued making measurements and generated some incorrect refractive index data. For those that have this type of instrument: is there a standard sample that we could run or tool parameters that we could check to ensure the health of the tool prior to making measurements?
Thanks for any advice you can provide!
Sandra G. Malhotra, Ph.D. | Technical Lab Manager
AggieFab Nanofabrication Facility
Department of Electrical & Computer Engineering, College of Engineering | Texas A&M University
3253 TAMU | College Station, TX 77843
ph: 979.845.3199 | s<mailto:hprichard at tamu.edu>andra.malhotra at tamu.edu<mailto:andra.malhotra at tamu.edu>
- - - - - - - - - - - - - - - - - - - - - - - -
TEXAS A&M UNIVERSITY | FEARLESS on Every Front
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20211020/9551e4b3/attachment.html>
More information about the labnetwork
mailing list