Dear colleagues,
I was wondering if anyone has experience with MBE growth of Neodymium and Praseodymium; I'd like to ask a few questions about the crucible's type (for growth in partial oxygen background), idle temperature for their effusion cells and safe handling of the materials.
As always I really appreciate your input.
Best regard,
Saba
--