We had our ellipsometer fixed about 2 years ago. I was in contact with Rusty at Gaertner:
Rusty
Gaertner Scientific Corporation
3650 Jarvis Ave
Skokie, IL 60076
TEL: 847 673 5006 email at GaertnerScientific.com<mailto:email at GaertnerScientific.com>
--
Rusty Kutko
Gaertner Scientific Corp.
3650 Jarvis Ave
Skokie(Chicago), IL 60076
Tel: 1 847 673 5006
Fax: 1 847 673 5009
Email: email at GaertnerScientific.com<mailto:email at GaertnerScientific.com>
Regards,
Carl Chow
Hewlett Packard Labs
From: labnetwork [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Vlahakis, James
Sent: Wednesday, September 15, 2021 2:32 PM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Gaertner Scientific contact?
Hi all, hope your semester is off to a good start (for those in the academic space).
We have a new to us Gaertner ellipsometer (thanks Vicky, Jim and Dan). Does anyone have contact info for Gaertner Scientific? I've reached out via the website - http://www.gaertnerscientific.com/main.htm<http://www.gaertnerscientific.com/main.htm> - multiple times but no response has been forthcoming and calls go directly to a generic voice mail box
jim
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210916/bc7c2aed/attachment.html>
More information about the labnetwork
mailing list