We have had very good success with the Solaris 150 RTA from SSI. We
have had this tool for over 10 years and it has been very reliable.
http://ssi-rtp.com/page/products/rtp-solaris-150/
Best Regards,
Brent
--
Brent P. Gila, PhD.
Associate Director, Research Service Centers
University of Florida
1041 Center Drive
Gainesville, Florida 32611
Tel:352-273-2245, Fax:352-846-2877
email: bgila at ufl.edu
On 4/6/2022 1:42 PM, Brian K. Olmsted wrote:
> *[External Email]*
>
> Hi,
>
> I'm looking at replacing an RTP-600S benchtop thermal processing unit
> and am looking for input and testimonials from others who may have a
> similar tool from a different vendor.
>
> I'm curious about others' experiences.
>
> Thanks much,
>
> Brian K. Olmsted
> Associate Director of Laboratory Operations
> University of Minnesota | MNC
> www.mnc.umn.edu
> <https://urldefense.proofpoint.com/v2/url?u=http-3A__www.mnc.umn.edu&d=DwMFaQ&c=sJ6xIWYx-zLMB3EPkvcnVg&r=gl_2fLZA_-_JfH_dOmx7ug&m=pM4UilKvx5cx6AYsmjCE8wAgCQVp6hiSjDRt6Chwa5GZikuRs33qFTI8qj2_qOaK&s=HmaomA6YGS42Ls__2sV2kOtWxlecrph3pKO7EHfA7lo&e=>
> 612.626.3287
> olms0025 at umn.edu
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://urldefense.proofpoint.com/v2/url?u=https-3A__mtl.mit.edu_mailman_listinfo.cgi_labnetwork&d=DwICAg&c=sJ6xIWYx-zLMB3EPkvcnVg&r=gl_2fLZA_-_JfH_dOmx7ug&m=pM4UilKvx5cx6AYsmjCE8wAgCQVp6hiSjDRt6Chwa5GZikuRs33qFTI8qj2_qOaK&s=E_TJ7LlTTcqPv_V75rC69IHvqRxR6WPGYrMDpdtdnR8&e=
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220407/0f8eb218/attachment.html>
More information about the labnetwork
mailing list