[labnetwork] Iridium sputter target?
Aebersold,Julia W.
julia.aebersold at louisville.edu
Wed Apr 20 11:30:22 EDT 2022
We were also asked to deposit iridium last year and the cost of the 3" target immediately stopped the project.
Cheers!
Julia Aebersold, Ph.D.
Manager, Micro/Nano Technology Center
University of Louisville
Shumaker Research Building, Room 233
2210 South Brook Street
Louisville, KY 40292
(502) 852-1572
http://louisville.edu/micronano/
From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Brian K. Olmsted
Sent: Tuesday, April 19, 2022 1:03 PM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Iridium sputter target?
CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.
Hi,
I've got a prospective customer interested in sputtering iridium. We don't have an iridium target and it probably doesn't make a lot of sense for us to purchase one for extremely limited interest/use. However, if there is another lab that has this capability I would be happy to steer them to you for at least this step in their process.
Any information or help is appreciated.
Thanks,
Brian K. Olmsted
Associate Director of Laboratory Operations
University of Minnesota | MNC
www.mnc.umn.edu<https://nam11.safelinks.protection.outlook.com/?url=http%3A%2F%2Fwww.mnc.umn.edu%2F&data=05%7C01%7Cjulia.aebersold%40louisville.EDU%7C4f913867e16e4490ad5208da2255449c%7Cdd246e4a54344e158ae391ad9797b209%7C0%7C0%7C637860046892720519%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C1000%7C%7C%7C&sdata=ICuT4PHPzPsTsBRbIAegatGo%2FFAg%2F0EKhkc5Vt0Uisk%3D&reserved=0>
612.626.3287
olms0025 at umn.edu<mailto:olms0025 at umn.edu>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220420/c369867c/attachment.html>
More information about the labnetwork
mailing list