[labnetwork] Iridium sputter target?
Thomas Daunais
tdaunais at hawksemiconductor.com
Wed Apr 20 13:34:24 EDT 2022
Hello Brian,
We can sputter iridium on substrates up to 150 mm and would be happy to
talk to your customer about their needs.
All the best,
--
*Thomas Daunais, PhD*
Lead process engineer
Hawk Semiconductor LLC
4108 Spring Lake Blvd.
Ann Arbor, MI 48108
hawksemiconductor.com
Ph: (231) 740-2720
On Wed, Apr 20, 2022 at 1:13 PM Aebersold,Julia W. <
julia.aebersold at louisville.edu> wrote:
> We were also asked to deposit iridium last year and the cost of the 3”
> target immediately stopped the project.
>
>
>
> Cheers!
>
>
>
> Julia Aebersold, Ph.D.
>
> Manager, Micro/Nano Technology Center
>
> University of Louisville
>
> Shumaker Research Building, Room 233
>
> 2210 South Brook Street
>
> Louisville, KY 40292
>
> (502) 852-1572
>
>
>
> http://louisville.edu/micronano/
>
>
>
> *From:* labnetwork <labnetwork-bounces at mtl.mit.edu> * On Behalf Of *Brian
> K. Olmsted
> *Sent:* Tuesday, April 19, 2022 1:03 PM
> *To:* labnetwork at mtl.mit.edu
> *Subject:* [labnetwork] Iridium sputter target?
>
>
>
> *CAUTION:* This email originated from outside of our organization. Do not
> click links, open attachments, or respond unless you recognize the sender's
> email address and know the contents are safe.
>
> Hi,
>
>
>
> I've got a prospective customer interested in sputtering iridium. We don't
> have an iridium target and it probably doesn't make a lot of sense for us
> to purchase one for extremely limited interest/use. However, if there is
> another lab that has this capability I would be happy to steer them to you
> for at least this step in their process.
>
>
>
> Any information or help is appreciated.
>
>
>
> Thanks,
>
>
> Brian K. Olmsted
>
> Associate Director of Laboratory Operations
>
> University of Minnesota | MNC
>
> www.mnc.umn.edu
> <https://nam11.safelinks.protection.outlook.com/?url=http%3A%2F%2Fwww.mnc.umn.edu%2F&data=05%7C01%7Cjulia.aebersold%40louisville.EDU%7C4f913867e16e4490ad5208da2255449c%7Cdd246e4a54344e158ae391ad9797b209%7C0%7C0%7C637860046892720519%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C1000%7C%7C%7C&sdata=ICuT4PHPzPsTsBRbIAegatGo%2FFAg%2F0EKhkc5Vt0Uisk%3D&reserved=0>
>
> 612.626.3287
>
> olms0025 at umn.edu
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220420/688a8180/attachment.html>
More information about the labnetwork
mailing list