[labnetwork] Lantanum evaporation
Alexey Kovalev
kovalev at magnet.fsu.edu
Wed Aug 17 11:34:06 EDT 2022
Hello All,
We are thinking about e-beam evaporation of Lanthanum.Kurt Lesker recommends either tungsten or tantalum liner and I am wondering what could be the difference in this case. I also found out that Thermionics thinks that alumina liner will work as well.
Could anybody please give a comment, either on evaporation of the lantanum, or on the liner material?
Thank you very much
Alexey
--
Alexey Kovalev
Assistant in Research
A302
NHMFL FSU
1800 E. Paul Dirac Dr.
Tallahassee , FL 32310-3706
kovalev at magnet.fsu.edu
TEL:850-644-0861
FAX:850-644-5038
5161 706C 6127