You may confuse the topic a bit. Those are general purpose crucibles. Once e-beam evaporation is mentioned, it is a pretty specific – and different - product type. While “crucible” is a common term used for those, “hearth liners” is a more precise one if confusion has to be avoided. Frankly speaking, even original question from Alexey used the term “liner”; my fault in switching to lab slang.
For example: https://thermionics.com/product-category/e-guns/crucible-liners/
And those have to be machined to a pretty precise dimension and surface finish, unlike regular furnace crucibles..
From: Ted Wangensteen <twangens at mail.usf.edu>
Sent: Friday, August 19, 2022 10:06
To: Michael Yakimov <yakimom at sunypoly.edu>
Cc: Alexey Kovalev <kovalev at magnet.fsu.edu>; labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Lantanum evaporation
Again, I have no experience with the chemistry, and perhaps usual places do not carry SiC.
However, I found this vendor - Perhaps something close to your size, or they can custom make something for your tool.
https://www.lmine.com/silicon-carbide-sic-crucibles-c-1_2_98/#:~:text=Silicon%20Carbide%20(SiC)%20Crucibles%20are,base%20metals%2C%20and%20other%20products.
Hope this might be helpful.
BR,
Ted
On Fri, Aug 19, 2022 at 8:59 AM Michael Yakimov <yakimom at sunypoly.edu<mailto:yakimom at sunypoly.edu>> wrote:
Are there commercially available SiC crucibles for e-beam? Never heard of those, and nothing at my usual suspects (Kamis, Lesker, Thermionics) nor on the first page of Google.
And there is certainly carbide formation in Al+SiC system at temperatures used for evaporation.
Iseki, T., Kameda, T. & Maruyama, T. Interfacial reactions between SiC and aluminium during joining. J Mater Sci 19, 1692–1698 (1984). https://doi.org/10.1007/BF00563067
________________________________
From: Ted Wangensteen <twangens at mail.usf.edu<mailto:twangens at mail.usf.edu>>
Sent: Friday, August 19, 2022 9:09:28 AM
To: Michael Yakimov <yakimom at sunypoly.edu<mailto:yakimom at sunypoly.edu>>
Cc: Alexey Kovalev <kovalev at magnet.fsu.edu<mailto:kovalev at magnet.fsu.edu>>; labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu> <labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>>
Subject: Re: [labnetwork] Lantanum evaporation
If C is a concern, you may consider SiC.
I have no experience with that, but you could research that type.
BR,
Ted Wangensteen
On Thu, Aug 18, 2022 at 7:19 PM Michael Yakimov <yakimom at sunypoly.edu<mailto:yakimom at sunypoly.edu>> wrote:
From the general perspective...
La is an active metal, it slowly oxidizes in the air. It is very feasible that it may react with carbon and form carbide, if melted in carbon crucible. So the way I read that crucible selection is "do not use carbon! Use something else". Yellow layer of Aluminum Carboide can become a problem with carbon crucible as well, so at least this is a feasible assumption.
As an active metal, again, it will wet most other crucibles - I don't think that can be avoided. Density of Liquid La is somewhat below solid, but not too much - so I suspect it may be breaking crucibles like Al, so beware of ceramic ones. Otherwise, I would be looking at crucible price - those materials must be steep.
If you have to justify the use of metal in evaporator, compare La with Al. It seem to be on the same page from e-beam deposition perspective.
Thanks
mike
-----Original Message-----
From: labnetwork <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> On Behalf Of dbouillez plasmaprocessgroup.com<http://plasmaprocessgroup.com>
Sent: Wednesday, August 17, 2022 17:26
To: Alexey Kovalev <kovalev at magnet.fsu.edu<mailto:kovalev at magnet.fsu.edu>>; labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Lantanum evaporation
Hello Alexey,
I have several questions if you don't mind me asking:
What gas environment do you intend to use for evaporation?
What is the end product you are looking to produce with the use of this material?
Are you looking for liners that allow for best adhesion of over spray? Or, looking at concerns with contamination from secondary deposition?
I can't say that I have a background on this material, but I would be interested in knowing the use for this material if it can be disclosed.
Thanks,
Dan
Dan Bouillez
Plasma Process Group
Sales
dbouillez at plasmaprocessgroup.com<mailto:dbouillez at plasmaprocessgroup.com>
PH 970-663-6988
Cell 970-415-7259
PPG business hours Mon-Thurs 7 am to 5:30pm Mountain time
-----Original Message-----
From: labnetwork <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> On Behalf Of Alexey Kovalev
Sent: Wednesday, August 17, 2022 9:34 AM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: [labnetwork] Lantanum evaporation
Hello All,
We are thinking about e-beam evaporation of Lanthanum.Kurt Lesker recommends either tungsten or tantalum liner and I am wondering what could be the difference in this case. I also found out that Thermionics thinks that alumina liner will work as well.
Could anybody please give a comment, either on evaporation of the lantanum, or on the liner material?
Thank you very much
Alexey
--
Alexey Kovalev
Assistant in Research
A302
NHMFL FSU
1800 E. Paul Dirac Dr.
Tallahassee , FL 32310-3706
kovalev at magnet.fsu.edu<mailto:kovalev at magnet.fsu.edu>
TEL:850-644-0861
FAX:850-644-5038
5161 706C 6127
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220819/71dd1fc7/attachment.html>
More information about the labnetwork
mailing list