Yb sublimates (like Cr). I've only ever thermally deposited it. Never
had any issues.
Joe
On 7/19/2022 8:52 PM, Chang, Long wrote:
> Hi all, a user wants to deposit Yb in our ebeam evaporator. Yb does not seem like a health hazard or adversely affects vacuum. It’s packed in oil, so is a bit complex to clean and load it while minimizing exposure to air. Does anyone have experience with Yb to share?
>
> Sent from my iPhone
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://nam12.safelinks.protection.outlook.com/?url=https%3A%2F%2Fmtl.mit.edu%2Fmailman%2Flistinfo.cgi%2Flabnetwork&data=05%7C01%7Cjpalmer%40princeton.EDU%7Cb06d2efb36ee476482f108da6a4654b7%7C2ff601167431425db5af077d7791bda4%7C0%7C0%7C637939147552652971%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C3000%7C%7C%7C&sdata=AzUWmU%2B%2BgKcIUbao8FtwvifnTw8U6rJktgPP%2Buw7AsQ%3D&reserved=0
--
Joseph E. Palmer
Chief of Operations for the MNFC
PIM, Princeton University
Contact:
Office: 609-258-4706
Cell: 609-731-8962
More information about the labnetwork
mailing list