[labnetwork] Microfabrication class
Eric Johnston
ericdj at seas.upenn.edu
Mon Oct 10 14:30:54 EDT 2022
Hi Sergi
We have done a soft lithography workshop for a while. A couple of things
that worked for us:
- Limit attendance to 6.
- Lecture is about 45 minutes, then we have a hand-on workshop that takes
about 3+ hours.
- We provide the mask, wafers, resist, and PDMS.
- We do not test the devices, which would take much too long.
- We charge for attendance, ~$50 per attendee. This was mostly to reduce
no-shows. Eventbrite makes it easy to sign up and to charge.
I can share my protocol and powerpoint if you like.
Best Regards
Eric
Eric Johnston
Interim Director
Quattrone Nanofabrication Facility
Singh Center for Nanotechnology
University of Pennsylvania
3205 Walnut Street, #116
ericdj at seas.upenn.edu
T. 215.573.6695
On Fri, Oct 7, 2022 at 3:38 PM Sergi Lendinez <sergilendi at lsu.edu> wrote:
> Dear labnetwork community,
>
>
>
> Here at LSU we are planning to start a microfabrication class soon, and I
> would like to ask for your opinions about setting up this kind of class at
> a university. I am not sure if this topic has been discussed here before,
> so I apologize for any possible duplication.
>
>
> Any information would be very helpful, like do's and don't's, devices
> being fabricated, number of students, students/teacher ratio, course load,
> etc.
>
>
> I'd like to fabricate some CMOS device, but we lack some critical
> equipment such as a diffusion tube furnace, cvd, or packaging tools, so I'm
> looking for alternate ideas: maybe a photodiode/detector, a Hall sensor or
> some micro-fluidic channels. If anyone has some experience fabricating
> these devices in a class setup, is there anything you'd be willing to share?
>
>
> Many thanks,
>
> Sergi
>
>
>
> *---*
>
> *Sergi Lendinez, Ph. D.*
> Assistant Director NFF | Louisiana State University
>
> Center for Advanced Microstructures and Devices (CAMD)
>
> 6980 Hefferson Highway, Baton Rouge, LA 70803
> (225) 578-9378
>
> sergilendi at lsu.edu | *lsu.edu/nanofabrication*
> <https://urldefense.com/v3/__https://lsu.edu/nanofabrication__;!!IBzWLUs!XghTGOjN4El_vJnH6I5fwfzt9SqdTyqCL-YzUbJoF8dokpSDKpQgVgP4r7QVnXIWK7uhkUaPmk8WYpHL9Bp-4WM$>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
>
> https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!IBzWLUs!XghTGOjN4El_vJnH6I5fwfzt9SqdTyqCL-YzUbJoF8dokpSDKpQgVgP4r7QVnXIWK7uhkUaPmk8WYpHLmAp5dC0$
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20221010/daf3ee57/attachment.html>
More information about the labnetwork
mailing list