[labnetwork] Fiji ALD factory reset
James Mitchell
jtmitch5 at ncsu.edu
Wed Oct 26 12:39:44 EDT 2022
I will look at ours to see if there is a default password. You could call
Veeco and ask.
Jim
On Wed, Oct 26, 2022 at 11:56 AM Bradash, Mihailo Rayko <mbradash at purdue.edu>
wrote:
> Hello,
>
>
>
> I was wondering if anyone who has experience with a Fiji ALD system would
> happen to know how to factory reset the software, or simply change the
> Engineering/Admin password?
>
> Our group no longer has access to what the password was originally set at
> and is needing to make changes to some of the layouts.
>
>
>
> Mihailo Bradash
>
> Research Engineer
>
> Purdue University
>
> Birck Nanotechnology Center
>
> 1205 W. State Street
>
> West Lafayette, Indiana 47907
>
> Office: (765)494-6522
>
> Cell: (219)670-4974
>
> mbradash at purdue.edu
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
--
*Thank you, Jim*
*James Mitchell*
*Specialty Trades Technician*
*Dept. of Electrical and Computer Engineering*
*North Carolina State University Nanofabrication Facility (NNF)*
*MRC RM243A **Box 7911*
*2410 Campus Shore Dr., Raleigh, NC 27606*
*jtmitch5 at ncsu.edu* <jtmitch5 at ncsu.edu>
*Desk: 919-515-5394*
*Cell: 919-717-7325*
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20221026/436e9097/attachment.html>
More information about the labnetwork
mailing list