I ran a quick calculation at your flow for a gas as heavy as propane in a ¼” ODT and it would be in the 2-5 PSI range. H2 pressure drop is under 1 PSID.
Often piping contractors like to use 3/8” as it is more rigid and pipe-like, easier to keep straight and does not need tubing supports as close together. This is especially true in longer tube runs where ¼” can show a visible “droop” .
John Boyle
John Boyle Consulting, LLC
4848 Canterbury Drive
Emmaus, PA 18049
484-432-7596 Cell
610-965-3208 Office
From: labnetwork [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Dennis Schweiger
Sent: Friday, September 02, 2022 5:45 AM
To: John Ransom
Cc: labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Stainless Steel Tubing
John,
Good morning. My rough guess is that 1/4" will be fine for your application, but without knowing the gas (density), and the delivery pressures, it's hard to give a definitive answer. The larger tubing size would give you a future margin for error if your process needs were ever to change, and using an HVCR fitting still gets you a connection that will work with the 1/4" VCR components.
One of the things you could consider is to deliver to the tools at a higher pressure, then step the pressure down at the tool with a mini regulator of some sort.
It's hard to provide a better answer without knowing more about your delivery system.
As always, if you want to discuss further, please feel free to give me a call.
Good luck,
Dennis Schweiger
University of Michigan/LNF
Facilities Supervisor
734.647.2055 Ofc
On Thu, Sep 1, 2022 at 5:25 PM John Ransom <jaransom at uark.edu> wrote:
I have gotten recommendations that I should use 3/8” SS tubing EP 316L, but the availability of that is out into May or June of 2023. ¼” is better.
But can I use ¼” with a process that runs <1slm? The fittings to most of the tools is ¼” VCR or swagelok. But I have a 90ft run in one case. Any guidance is appreciated.
John Ransom
Program Manager – MUSiC Facility
Multi-User SiC Fabrication Facility
University of Arkansas
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220902/86c4e655/attachment.html>
More information about the labnetwork
mailing list