[labnetwork] Treating silane exhaust from PECVD
Iulian Codreanu
codreanu at udel.edu
Thu Jan 12 17:27:08 EST 2023
Hi Hadi,
I've been using dry, resin-based scrubbers provided by Jupiter
Scientific. They are relatively small, affordable, and easy to
operate/maintain.
Cheers,
Iulian
iulian Codreanu, Ph.D.
Director, Nanofabrication Facility
University of Delaware
Harker ISE Lab, Room 163
221 Academy Street
Newark, DE 19716
302-831-2784
http://udnf.udel.edu
On 1/12/2023 2:35 PM, Hadi Esmaeilsabzali wrote:
>
> Dear Colleagues,
>
> For those who run PECVD at their facilities, I am wondering how you
> process the exhaust from your systems.
>
> We used to treat the PECVD exhaust along with that of the SiNx tube
> furnace through a TPU. We have recently decommissioned our furnace
> and TPU as they were too costly to run and are looking at alternative
> exhaust options for the PECVD only. We use our PECVD tool for oxide
> and nitride deposition, and it's worth noting that it only uses silane
> (no ammonia).
>
> Some colleagues had mentioned that they don't use a TPU/scrubber and
> send the process waste to the building exhaust (untreated). Given that
> our PECVD processes use a relatively small silane flow (~30 sccm for
> up to 30 mins per run each week - all max values) and it is
> significantly diluted, this sounded a practical option.I am trying to
> see if others have tried or can comment on this approach,
> particularly for a silane-based PECVD process. Aside from the
> flammability concerns, we are also aware of the potential oxide
> buildup in the exhaust system over time.
>
> I appreciate it if you share other (cost-effective) suggestions you
> might have for us!
>
> Thanks,
> Hadi
>
> *Hadi Esmaeilsabzali, PhD*
>
> Nanofabrication Group Manager, 4D LABS
>
> Simon Fraser University
>
> 8888 University Dr., Burnaby, B.C. V5A 1S6
> T: 778.782.3790 | F: 778.782.3765| www.4dlabs.ca <http://www.4dlabs.ca/>
> Facebook <https://www.facebook.com/4dlabs/> | Twitter
> <https://twitter.com/4D_LABS> | LinkedIn
> <https://www.linkedin.com/company/sfu-4d-labs/about/>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230112/b8c3f0f8/attachment.html>
More information about the labnetwork
mailing list