HI James,
Given the long lead time, why don't you try simply checking the voltage outputs from the linear regulator if that seems fine, try changing the socketed semiconductors chips without getting into the effort of testing each one (it saves time). Also replace any electrolytic capacitors if this unit is over 5-7 year old. Also look for any obvious sign of component damage or burn out/degradation.
Warm Regards
Rohit Khanna
Electronic Test & Measurement Engineer
London Centre for NANO Technology, UCL
Ph:+44-020-76799984
Lab: +44 20 3108 1516
Int Ext: 39984
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Charles Veith <cveith at seas.upenn.edu>
Sent: 14 June 2023 21:13
To: James Grant <James.Grant at glasgow.ac.uk>
Cc: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Control Board OIPT Plasmalab System 100
⚠ Caution: External sender
Hi James
What is the cost they are quoting you for the board? If the price is significant, maybe think about buying a system at auction
and cannibalizing it. Today I received an email about a large auction occurring soon and you might get lucky this way.
Regards,
Charlie
On Wed, Jun 14, 2023 at 3:43 PM James Grant <James.Grant at glasgow.ac.uk<mailto:James.Grant at glasgow.ac.uk>> wrote:
Hello,
The AMU on our OIPT Plasmalab System has been playing up. OIPT reckon the solution is either to replace the AMU control card or the whole board but are quoting a lead time of 365 days (!).
[cid:188bb87de024cff311]
Does anyone have a spare?
AMU card part number = PC00S26875
Board part number = MA00Z26876
Cheers,
James
Dr. James Paul Grant
Research Engineer in Plasma Processing
Plasma Processing Group
james.grant at glasgow.ac.uk<mailto:james.grant at glasgow.ac.uk>
[cid:188bb87de025b16b22]
www.JWNC.gla.ac.uk<https://urldefense.com/v3/__http://www.jwnc.gla.ac.uk/__;!!IBzWLUs!X6X4B8YXoiHuYJgQ-ObItB8DFbxRojsGyNbVYiX-9ZFMVcSb_f-ZesR76GIz3yUijjYI3uIvuHKnaXoatZ4_nz4uRW9aMw$>
[cid:188bb87de02692e333] LinkedIn.com/company/JWNC<http://linkedin.com/company/JWNC>
[cid:188bb87de027745b44] @UofG_JWNC<https://urldefense.com/v3/__https://twitter.com/uofg_jwnc__;!!IBzWLUs!X6X4B8YXoiHuYJgQ-ObItB8DFbxRojsGyNbVYiX-9ZFMVcSb_f-ZesR76GIz3yUijjYI3uIvuHKnaXoatZ4_nz4JT6f5pg$>
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!IBzWLUs!X6X4B8YXoiHuYJgQ-ObItB8DFbxRojsGyNbVYiX-9ZFMVcSb_f-ZesR76GIz3yUijjYI3uIvuHKnaXoatZ4_nz7XgWTIYg$
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230615/5d356fa0/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 2023700 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230615/5d356fa0/attachment.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image002.png
Type: image/png
Size: 26666 bytes
Desc: image002.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230615/5d356fa0/attachment-0001.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image003.png
Type: image/png
Size: 1538 bytes
Desc: image003.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230615/5d356fa0/attachment-0002.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image004.png
Type: image/png
Size: 1717 bytes
Desc: image004.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230615/5d356fa0/attachment-0003.png>
More information about the labnetwork
mailing list