[labnetwork] Heidelberg MLA150 SU-8 Exposure Dose
Michael Yakimov
yakimom at sunypoly.edu
Fri Jun 23 11:15:06 EDT 2023
375 looks to be in the region where both native absorbtion and exposure bleaching are significant, and absorbtion curve sliope is high. .
An interesting experiment I see is a measurements of transmitted light intensity during exposure. If you can do that, I suspect that may give a lot of food for though.
THanks
mike
_______________________________________________
Michael Yakimov
Research scientist
College of Nanoscale Science and Engineering
SUNY Polytechnic Institute
253 Fuller rd.
Albany NY 12203
Phone: 518-437-8609 lab
e-mail: yakimom at sunypoly.edu
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Hollingshead, Dave <hollingshead.19 at osu.edu>
Sent: Thursday, June 22, 2023 1:28:43 PM
To: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: [labnetwork] Heidelberg MLA150 SU-8 Exposure Dose
Dear Labnetwork,
We have found that exposure of SU-8 on our MLA150 tool (using the 375nm laser) seems to require very high doses. Even thin ~500nm thick films (using SU-8 2000.5) have required doses on the order of 1200mJ/cm2 to fully expose. This is 15-20x the recommended dosage from both the datasheet and what we estimate is the exposure dose used on our filtered contact aligners. Thicker films follow the same trend, but not necessarily in a linear fashion (5µm films require ~2000mJ/cm2).
I am sure the bump from 365nm to 375nm plays a role, but the magnitude of the change seems excessive. FWIW, our other negative resists (eg. nLOF2020) seem to expose properly at reasonable doses.
Has anyone else experienced this? Does anyone have an explanation or any processing suggestions for using SU-8 with an MLA?
Thanks,
-Dave
Dave Hollingshead
Manager, Research Operations
The Ohio State University
Nanotech West Labs
Suite 100, 1381 Kinnear Rd, Columbus, OH 43212
614.292.1355 Office
hollingshead.19 at osu.edu<mailto:hollingshead.19 at osu.edu> / nanotech.osu.edu<http://nanotech.osu.edu>
Pronouns: he/him/his
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230623/427eb7de/attachment.html>
More information about the labnetwork
mailing list