[labnetwork] fiji G2 Loading
Bas van Asten
B.vanAsten at tudelft.nl
Wed Sep 13 03:12:15 EDT 2023
Dear Peter,
Yes, we have a Fiji G2 system with automatic hline loader.
We have problems loading the system every once in a while.
It's important to make sure the operators check that the sample plate is touching the prong base completely before loading.
If else over time it can move further and further out.
Best regards,
B. van Asten
Process Engineer
TU Delft
Faculty Applied Sciences
Lorentzweg 1
2628 CJ Delft
T +31 6 424 81091
E B.vanAsten at tudelft.nl<mailto:B.vanAsten at tudelft.nl>
Available on weekdays
From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Peter Lomax
Sent: Tuesday, September 12, 2023 5:57 PM
To: Fab Network <labnetwork at mtl.mit.edu>
Subject: [labnetwork] fiji G2 Loading
Hello all,
Has anybody got a Fiji G2 ALD, if so have you had any issues with the loading system.
Cheers
Peter
Sent from Outlook for iOS<https://urldefense.com/v3/__https:/aka.ms/o0ukef__;!!PAKc-5URQlI!8uDPAL94oEZ8WDD0STosnAAa7_cdSFKtHGFgU34XX-RaD94-aT5IyuqDCPO14GdhtYKTeH2P5P58jrpiW91QUFPtEUM$>
The University of Edinburgh is a charitable body, registered in Scotland, with registration number SC005336. Is e buidheann carthannais a th' ann an Oilthigh Dhùn Èideann, clàraichte an Alba, àireamh clàraidh SC005336.
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230913/d5cdd838/attachment.html>
More information about the labnetwork
mailing list