[labnetwork] HMDS lifetime in YES oven
Martin, Michael
michael.martin at louisville.edu
Fri Apr 12 16:37:22 EDT 2024
To Bill's point (from Florida), same here. Our HMDS in the YES oven is probably 10 years old and qualitatively still works. It makes our substrates hydrophobic and resist adhesion is good though we are not using a goniometer to verify the contact angle.
-Michael
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Zhichao Wang <zhichaow at udel.edu>
Sent: Monday, April 8, 2024 5:40 PM
To: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: [labnetwork] HMDS lifetime in YES oven
CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.
Dear Lab Network,
I was wondering how long the lifetime is for the HMDS in the YES oven. On the note from the YES's website, it says " If the HMDS is more than a year old, it should probably be replaced". I would assume the "year" here starts from the HMDS manufactured date, which is the shelf life for a brand new bottle of HMDS. Do you guys have experience on using the HMDS for extended time (like 6+ months) after the expiration date? Please let me know your thoughts and suggestions. Many thanks!
Best,
Chao
--
[https://ci3.googleusercontent.com/mail-sig/AIorK4x_Y6s1D-QRl-0PHmw-IKysmBp1Gr83JeY3kMWLc6K2VhCqyd-PX_9Jh3QjaDEpSxLygmnUyHk]
Zhichao "Chao" Wang, Ph.D.
Lithography Engineer
UDNF
University of Delaware
Pronouns: He/Him/His
------------------------
Office Number:(302) 831-4839
221 Academy St.,RM170
Newark, DE 19711
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240412/4e3560fb/attachment.html>
More information about the labnetwork
mailing list