[labnetwork] Precious Metal Reclaim Service
Iulian Codreanu
codreanu at udel.edu
Mon Mar 25 16:58:07 EDT 2024
I use Glines and Rhodes.
iulian Codreanu, Ph.D.
Director, Nanofabrication Facility
University of Delaware
Harker ISE Lab, Room 163
221 Academy Street
Newark, DE 19716
302-831-2784
https://udnf.udel.edu
On 3/4/2024 1:04 PM, Chang, Long wrote:
> Hi All,
>
> Who do you use for precious metal reclaiming from spent targets and
> chamber/shield scraping?
>
> Thanks,
> Long Chang
> UH Nanofabrication Facility
> Houston, TX
> lvchang at central.uh.edu
>
>
>
>
>