Velasquez-Garcia Group's 3D-Printed Device Builds Better Nanofibers

October 30, 2017

Printed nozzle system could make uniform, versatile fibers at much lower cost.

MIT-Regular-Nanospinners-01_0.jpg
A 3-D-printed manufacturing device can extrude fibers that are only 75 nanometers in diameter, or one-thousandth the width of a human hair.

Image: Luis Fernando Velásquez-García


Read full story here.