Hello all,
Recently when discussing with Bill Flounders about adding a surfactant to
BHF solution he suggested to use Triton X-100.
We like to use it in a diluted form. From internet I could find water,
toluene, xylene and ethanol can be used as diluent. However water may turn
the solution gelatinous.
Does anyone have experience with diluting triton x-100 (supplier Sigma
Aldrich)?
Thanks,