[labnetwork] special wafers
David A. Bunzow
dabunzow at lbl.gov
Fri Oct 26 10:48:54 EDT 2012
Matthieu,
Not sure of your other technical specs for these ~double-thick wafers, so this
may sound off the wall.
Have you considered wafer bonding to create such a structure?
David A. Bunzow
User Facilities Program Manager
The Molecular Foundry
Materials Science Division
Lawrence Berkeley National Laboratory
1 Cyclotron Road MS 67-3207
Berkeley, CA 94720
Office: 510-486-4574
FAX: 510-486-7424
Cell: 510-542-1747
On 10/26/2012 4:55 AM, Matthieu Nannini, Dr. wrote:
> Dear colleagues,
>
> I'm looking for specific kinds of wafers: 150mm DSP Si 1.2mm thick. I already tried a few suppliers (Addison, WRS and University Wafers) but all have lead time of 8 weeks or so.
> Would any of you know suppliers that could have this kind of wafers ?
>
> Thanks
>
>
> -----------------------------------
> Matthieu Nannini
> McGill Nanotools Microfab
> Manager
> t: 514 398 3310
> c: 514 758 3311
> f: 514 398 8434
> http://mnm.physics.mcgill.ca/
> ------------------------------------
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20121026/c44d513e/attachment.html>
More information about the labnetwork
mailing list