[labnetwork] KOH Baths
Steve Franz
franz at seas.ucla.edu
Fri Dec 13 16:02:19 EST 2013
Hi Bill
At UCLA we pour as needed. Volume is usually enough for 1 or 2 wafers
as none of our customers need batch etching.
Regards
Steve Franz, Manager NRF
franz at seas.ucla.edu
310-206-8923
On Dec 13, 2013, at 10:06 AM, Bill Flounders wrote:
> Lab Network,
> Do any members maintain a standing KOH (30% or other) etch bath;
> or do you primarily support individual preparation and use?
> Thank you for a brief description of your policy or strategy here.
> Sincerely,
> Bill Flounders
> UC Berkeley
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20131213/17bfa64f/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: PastedGraphic-2.tiff
Type: image/tiff
Size: 33336 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20131213/17bfa64f/attachment.tiff>
More information about the labnetwork
mailing list