[labnetwork] KOH Baths
Flückiger Philippe
philippe.fluckiger at epfl.ch
Sat Dec 14 02:17:43 EST 2013
Dear Bill,
We operate 2 recirculating KOH baths permanently installed (23%@90°C & 40%@60°C) :
- http://cmi.epfl.ch/etch/PladeKOH.php#description
With my very best regards,
Philippe
Dr Philippe Flückiger
Director of Operations
http://cmi.epfl.ch/
Phone +41 21 693 6695
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Bill Flounders
Sent: 13 December 2013 19:07
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] KOH Baths
Lab Network,
Do any members maintain a standing KOH (30% or other) etch bath; or do you primarily support individual preparation and use?
Thank you for a brief description of your policy or strategy here.
Sincerely,
Bill Flounders
UC Berkeley
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20131214/fd1846a5/attachment.html>
More information about the labnetwork
mailing list