[labnetwork] KOH Baths
Aebersold,Julia W.
julia.aebersold at louisville.edu
Mon Dec 16 10:34:40 EST 2013
We also keep our bath at ambient temps until it is needed and then it is heated upon demand.
Cheers!
Julia Aebersold, Ph.D.
MNTC Cleanroom Manager
Shumaker Research Building, Room 233
2210 South Brook Street
University of Louisville
Louisville, KY 40292
502-852-1572
http://louisville.edu/micronano/
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Fouad Karouta
Sent: Friday, December 13, 2013 6:05 PM
To: Bill Flounders; labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] KOH Baths
Hi Bill,
We decided a year to get a standing KOH bath (don't recall the supplier name however in US). If unused it is at room temperature and heating to 70-80C is quite fast for usage. We believe it is safer this way as users do not need to make the KOH mixtures which include some hazards. We also monitor regularly the pH of the solution and top up KOH whenever required.
Kind regards, Fouad
________________________________________
From: labnetwork-bounces at mtl.mit.edu [labnetwork-bounces at mtl.mit.edu] on behalf of Bill Flounders [bill at eecs.berkeley.edu]
Sent: 14 December 2013 05:06
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] KOH Baths
Lab Network,
Do any members maintain a standing KOH (30% or other) etch bath; or do you primarily support individual preparation and use?
Thank you for a brief description of your policy or strategy here.
Sincerely,
Bill Flounders
UC Berkeley
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
More information about the labnetwork
mailing list