[labnetwork] question about resizing 200mm wafers down to 100mm
Michael Khbeis
khbeis at uw.edu
Tue Mar 12 17:15:56 EDT 2013
Benes,
From June 2011:
Questech Services Corp
2201 Executive Drive
Garland TX 75041-6120
972-278-8006
We ran laser downsize from 8" to 6", with bevel, semi-standard flat, edge grinding, photoresist, and laser marking.
Good luck,
Dr. Michael Khbeis
Associate Director
Microfabrication Facility (MFF)
University of Washington
Fluke Hall, Box 352143
(O) 206.543.5101
(F) 206.221.1681
(C) 443.254.5192
khbeis at uw.edu
http://www.engr.washington.edu/mff/
On Mar 12, 2013, at 6:50 AM, Benes Zdenek wrote:
> Hi,
>
> terribly sorry for this unsolicited email, but would any of you know a good reference for a company, that does wafer resizing from 200mm to 100mm wafers? ideally 2 small wafers from one large one, they would also apply protective resist coating on both sides, and round the edges afterwards?
>
> preferably, on the Swiss side of the Atlantic ocean :-)
>
> thanks a lot for the tips
>
> sincerely
>
> zdenek
>
> --------------------------------------------
> Zdenek Benes, PhD
> Ebeam, SEM, FIB engineer
> Center of MicroNanoTechnology, EPFL
>
> BM 1.127 (BM Building)
> Station 17
> CH-1015 Lausanne
> Switzerland
>
> Phone: +41 21 693 7751
> Fax: +41 21 693 5770
> Email: zdenek.benes at epfl.ch
>
> CMI : http://cmi.epfl.ch/
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
A non-text attachment was scrubbed...
Name: smime.p7s
Type: application/pkcs7-signature
Size: 1366 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20130312/da024327/attachment.bin>
More information about the labnetwork
mailing list