[labnetwork] question about resizing 200mm wafers down to 100mm
Pramod C Karulkar
pkarulkar9 at gmail.com
Tue Mar 12 18:28:19 EDT 2013
A company in Pasadena, California, Crystal Mark, sold a small machine
to do this. They used to do service. See: Wafer Coring and contouring
at http://www.crystalmarkinc.com/applications/water-processing
Normally the job involves going from a larger diameter (8" or 6") to
smaller diameter (6', 4" or 3"). Getting two tiny wafers from one
large wafer might be difficult on a lathe-like machine that is normally
used for this kind of job. However, it is not impossible. You may
have to develop a jig specific to your needs.
Good luck.
Pramod Karulkar
Pramod C Karulkar Ph. D.
Home 2*5*3* 3*0*3 0*4*1*8
6024 33rd Street Ct NW
Gig Harbor WA 98335
<http://www.crystalmarkinc.com/applications/water-processing>
On 3/12/2013 6:50 AM, Benes Zdenek wrote:
> Hi,
>
> terribly sorry for this unsolicited email, but would any of you know a
> good reference for a company, that does wafer resizing from 200mm to
> 100mm wafers? ideally 2 small wafers from one large one, they would
> also apply protective resist coating on both sides, and round the
> edges afterwards?
>
> preferably, on the Swiss side of the Atlantic ocean :-)
>
> thanks a lot for the tips
>
> sincerely
>
> zdenek
>
> /--------------------------------------------/
> /Zdenek Benes, PhD/
> /Ebeam, SEM, FIB engineer/
> /Center of MicroNanoTechnology, EPFL/
> /
> /
> /BM 1.127 (BM Building)
> Station 17
> CH-1015 Lausanne
> Switzerland
>
> Phone: +41 21 693 7751
> Fax: +41 21 693 5770
> Email: zdenek.benes at epfl.ch
>
> CMI : http://cmi.epfl.ch//
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
--
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20130312/d03e9f80/attachment.html>
More information about the labnetwork
mailing list