Xiaojin,
I had to get parts for my SRD. There are two companies that have parts.
Sitek Process Solutions
233 Technology Solutions
Rocklin, CA 95765
916-797-9000
OEMgroup East Inc
416 S 4th Street
Coopersburg, PA 18031
610-282-0105 x246
Gail Adams
Hope this helps,
Henry Taylor
On Thu, Jul 31, 2014 at 3:20 PM, Wang,Xiaojin <xiaojin.wang at louisville.edu>
wrote:
> Dear colleagues:
>
>
>
> We have a spin rinse dryer from semitool that has been down lately. After
> I discussed with technical support several times, the problem boil down to
> the motor controller whose part number is 60710-27. The picture is
> attached. Does anyone know where to repair this part besides OEM? Or does
> anyone have an old working one that we can purchase? Thank you.
>
>
>
> Xiaojin Wang
>
> Senior micro/nano process engineer
>
> Micro/nano technology center
>
> University of Louisville
>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20140801/704ba38e/attachment.html>
More information about the labnetwork
mailing list