Hello Ian,
Two of our service engineers are former STS employees (a good solution when you have 10 STS tools - the oldest dating back to 1993). They won't mind answering a question or two, so if you have any, drop me a line.
Several of the "old school" service engineers are now freelance. For a year 2000 system, I'm told that Gareth Morgan could be a good call. He has setup his own company based in the UK and is willing to travel - <gareth.morgan at homecall.co.uk>
Best regards,
Leif
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Ian Harvey
Sent: 12. august 2014 23:14
To: Matthieu Nannini
Cc: labnetwork at mtl.mit.edu
Subject: [labnetwork] And STS too… Re: Alcatel/Tegal DRIE support
Dear Mathieu and colleagues
We have the same question about STS... Who do you call when you run out of troubleshooting ideas on a 2000-vintage STS DRIE?
Thanks,
—Ian
Utah Nanofab / University of Utah
Micron Technology Foundation Inc., Microscopy Suite Sorenson Molecular Biotechnology Building — A USTAR Innovation Center
On Aug 12, 2014, at 1:21 PM, Matthieu Nannini wrote:
Dear colleagues,
For those of you who own an Alcatel/Tegal DRIE, where do you get support from ? Our service guy (former Alcatel Eng. in France) is hard to get a hand on.
Thanks
Matthieu
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
More information about the labnetwork
mailing list