Hello everyone,
We have a new lab member who needs sputtered Zn for his project. Do any of
your labs have experience with sputtering Zn?
We know that Zn sublimes easily in vacuum and thus poses a
cross-contamination risk. I'd greatly appreciate any advice or comments on
the advisability of introducing Zn into a sputterer shared with other
materials, and/or suggestions for techniques to avoid cross-contamination.
Thanks so much for your help,
Nadine
--