Forgot to mentioned , dress code and bringing stuff from other areas with more contaminants requirements also plays a big part.. Regards
Sent from my iPhone. Mario A. Portillo. High' born Technology USA
> On Aug 5, 2015, at 3:52 PM, hbtusainc <hbtusainc at yahoo.com> wrote:
>
> Richard , I have done extensive work in wafer foundries worldwide, for that size of cleanroom space 3-4 people is the max to keep the cleanliness at all times .. Anybody that needs to come into those modules is required to do a head count before coming in.
>
> I hope this helps , regards ...
>
> Sent from my iPhone. Mario A. Portillo. High' born Technology USA
>
>> On Aug 5, 2015, at 11:37 AM, Morrison, Richard H., Jr. <rmorrison at draper.com> wrote:
>>
>> HI,
>>
>> Is there a rule of thumb that is used to set a maximum capacity (# of people) in a cleanroom. I have class 10 rooms that are only 360 sqft with 450 air changes per hour and if I have >3 people in the space I have issues with particle control.
>>
>> Any ideas on maximum capacity in a room by class?
>>
>> Thanks
>> Rick
>>
>>
>> Draper Laboratory
>> Principal Member of the Technical Staff
>> Group Leader Microfabrication Operations
>> 555 Technology Square
>> Cambridge Ma, 02139-3563
>>
>> www.draper.com
>> rmorrison at draper.com
>> W 617-258-3420
>> C 508-930-3461
>>
>> Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper Laboratory. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
>> _______________________________________________
>> labnetwork mailing list
>> labnetwork at mtl.mit.edu
>> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20150805/2ab56ce2/attachment.html>
More information about the labnetwork
mailing list