We purchase 1 liter containers of AZ5214E positive resist from Integrated
Micro Materials. A one liter container is $685. Developer is $84 per
case, 4x4L. Plus ~$150 for shipping. The contact information is as follows:
Integrated Micro Materials
8141 Gateway Dr, Ste 240
Argyle, TX 76226
888-632-0997 Phone
940-228-2234 Fax
Customerservice at imicromaterials.com
Best Regards
Neil
On Jan 30, 2015 1:11 PM, "Peters, Michael S" <michael.peters at mnsu.edu>
wrote:
> Our EE cleanroom is looking to reduce the amount of photoresist we have
> to dispose of due to its age. We have, over the past 10-12 year, been
> receiving a generous donation of HPR-504 positive photoresist, developer
> and stripper all in gallon containers. The developer and stripper are used
> in its donated quantities, however, the photoresist we use less than a pint
> in a 2 year span. This leaves us over ¾ of a gallon to dispose of as
> chemical waste which negates the benefit of the donation. Our EHS would
> like us to see it there is a way to get the resist in smaller quantity to
> reduce the cost of disposal.
>
>
>
> I would appreciate a source where I could get smaller amounts of the photo
> resist.
>
>
>
> Thanks
>
>
>
> Mike Peters
>
> Engineering Specialist Sr.
>
> Radiation Safety Officer
>
>
>
> Minnesota State University, Mankato
>
> 141 Trafton Science Center North
>
> Mankato, Minnesota 56001
>
>
>
> Telephone: *507-389-1026 <507-389-1026>*
>
> Email: * michael.peters at mnsu.edu <michael.peters at mnsu.edu>*
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20150130/52ce924e/attachment.html>
More information about the labnetwork
mailing list