[labnetwork] Ni evaporation
Nava Ariel- Sternberg
anava at tauex.tau.ac.il
Mon Mar 23 05:30:06 EDT 2015
Hi all,
We've came across some issues with Ni e-beam evaporation and thought of consulting the network:
Which crucible are you using for Ni e-beam evaporation? We've tried Al2O3 and Vitreous carbon, both recommended by the material/crucible suppliers.
Any tips with respect to melting the material or the evaporation process itself?
Thanks,
Nava