Hello Nava,
Dr. Gerard Henein is our PVD expert and responsible for our evaporators. He uses a copper crucible for Ni.
Gerard is copied if you want to follow up with him.
Best,
Vince
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Nava Ariel- Sternberg
Sent: Monday, March 23, 2015 5:30 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Ni evaporation
Hi all,
We've came across some issues with Ni e-beam evaporation and thought of consulting the network:
Which crucible are you using for Ni e-beam evaporation? We've tried Al2O3 and Vitreous carbon, both recommended by the material/crucible suppliers.
Any tips with respect to melting the material or the evaporation process itself?
Thanks,
Nava
Nava Ariel-Sternberg, Ph.D.
Tel-Aviv University Center for Nanoscience and Nanotechnology, Managing Director
MNCF Manager
Phone: 03-640-5619
Mobile: 054-9984959
Email: anava at tauex.tau.ac.il<mailto:anava at tauex.tau.ac.il>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20150323/b8346d6d/attachment.html>
More information about the labnetwork
mailing list