Hello Nava,
In my lab we do not use a crucible. We put the Ni pellets directly in the
hearth. The Ni melts into a ball. It does not stick to the hearth.
Best,
Henry Taylor
Senior Hardware Engineer
NNF at NCSU
On Mon, Mar 23, 2015 at 5:30 AM, Nava Ariel- Sternberg <
anava at tauex.tau.ac.il> wrote:
> Hi all,
>
>
>
> We've came across some issues with Ni e-beam evaporation and thought of
> consulting the network:
>
>
>
> Which crucible are you using for Ni e-beam evaporation? We've tried Al2O3
> and Vitreous carbon, both recommended by the material/crucible suppliers.
>
> Any tips with respect to melting the material or the evaporation process
> itself?
>
>
>
> Thanks,
>
>
>
> Nava
>
>
>
>
>
> Nava Ariel-Sternberg, Ph.D.
>
> Tel-Aviv University Center for Nanoscience and Nanotechnology, Managing
> Director
>
> MNCF Manager
>
> Phone: 03-640-5619
>
> Mobile: 054-9984959
>
> Email: anava at tauex.tau.ac.il
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20150323/f944a5b4/attachment.html>
More information about the labnetwork
mailing list