I agree, never had a problem with Ni sticking. It is also fun to note
the change in the beam shape when the Ni source goes above its Curie point.
Regards,
Mark K Mondol
On 3/23/2015 10:03 AM, Henry Taylor wrote:
> Hello Nava,
>
> In my lab we do not use a crucible. We put the Ni pellets directly in
> the hearth. The Ni melts into a ball. It does not stick to the hearth.
>
> Best,
> Henry Taylor