Because it can build up pressurized gas, it is shipped with a pressure
release cap. The cap can leak and nanostrip will attack the paper labels.
If enough gets out it could attack the box it is shipped in. Make sure that
it does not sit on the loading dock and get warm. Our driver drops our
chemicals off first so we usually don't have this issue. If it sits on the
hot truck for a long period, you can get leaking.
Rob
On Wed, Nov 2, 2016 at 11:28 PM, Shivakumar Bhaskaran <bshiva at stanford.edu>
wrote:
> Mason,
>
>
> Nanostrip I used to buy comes with plastic container. I haven’t had any
> issue in storing for long period of time. I buy from Capitol Scientific (Cyantek®
> KMG Nano-Strip 2X®). Sometimes you may need to have different cap on the
> lid which might remove the buildup pressure from the Nanostrip. -Shiva
>
>
>
>
>
>
>
>
>
> *From:* labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces@
> mtl.mit.edu] *On Behalf Of *Mason Risley
> *Sent:* Wednesday, November 2, 2016 9:17 AM
> *To:* labnetwork at mtl.mit.edu
> *Subject:* [labnetwork] Nanostrip Storage Container
>
>
>
> All,
>
>
>
> Has anyone experienced problems with storing nanostrip solution (a
> stabilized form of piranha)? We recently purchased a gallon of it, the
> first shipment did not arrive due to “damaged packaging during shipment”
> the second round did in fact arrive but the bottle itself (which is just a
> plastic HDPE 4L chemical bottle) appears to be degrading, chemical label is
> completely gone and the plastic lining is – is this something that can be
> stored in a glass container? It seems interesting that something
> specifically engineered and used for dissolving organics and removing
> polymers is stored in a plastic container.
>
>
>
> Thanks,
>
>
>
> *Mason Risley*
>
> *Process Development Engineer*
>
> *Carnegie Mellon University Nanofabrication *
>
> 5000 Forbes Street, Pittsburgh PA 15213
>
> nanofab-staff at lists.andrew.cmu.edu | http://www.nanofab.ece.cmu.edu/
>
> ph: 412.268.5419 | cell : 505.795.4805
>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
>
--
Robert W. Hower, Ph.D.
The University of Michigan, Lurie Nanofabrication Facility
1301 Beal Ave, 1234A EECS
Ann Arbor, MI 48109
734-827-4370
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20161103/4df19642/attachment.html>
More information about the labnetwork
mailing list