[labnetwork] Sputter VO2 and V2O5
Fouad Karouta
fouad.karouta at anu.edu.au
Tue Aug 1 19:39:55 EDT 2017
Dear all,
As explained in below email we opted not to use VO2 in our multi-targets sputter system.
However I wonder if any facility in the network does have a dedicated sputter capability for VO2 and V2O5 (reactive).
Thanks,
Fouad Karouta
From: Fouad Karouta
Sent: Monday, 15 May 2017 9:47 AM
To: 'labnetwork at mtl.mit.edu' <labnetwork at mtl.mit.edu>
Subject: Sputter V, VO2
Dear network,
We have an AJA sputter system with over 50 different targets. It is a multi-users facility and we do change targets 2-3 times per week. To minimise possible cross-contamination every target has its own mounting accessories (housing, chimney, etc).
My question relate to possible toxic by-products and we like to share this topic within this network looking to hear your experience with same targets or targets that may produce toxic/dust by-products.
So recently we purchased Vanadium and Vanadium oxide VO2 targets. Our user intends to use reactive sputtering to produce different stoichiometry of the alloys. We found that some forms of vanadium oxide are toxic like V2O4 and V2O5 (highly toxic and poisonous, especially the dust and fumes).
So we like to share the following questions/remarks and we appreciate your comments:
1- Does someone use targets that may produce such toxic by-products, and how you handle this in a multi-user facility?
2- Outside an adequate mask + filters do you take any other precautions when opening chamber to change targets?
3- After the use of such targets with the potential risk of toxic particles would a sputtering a thin layer of an Al or Cr layer would cover the toxic particles and form a possible alternative to this issue?
Thank you,
Fouad Karouta
*************************************
Manager ANFF ACT Node
Australian National Fabrication Facility
Research School of Physics and Engineering
L. Huxley Building (#56), Mills Road, Room 4.02
Australian National University
ACT 0200, Canberra, Australia
Tel: + 61 2 6125 7174
Mob: + 61 451 046 412
Email: fouad.karouta at anu.edu.au<mailto:fouad.karouta at anu.edu.au>
http://anff-act.anu.edu.au/
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20170801/94091d94/attachment.html>
More information about the labnetwork
mailing list