Hello Mathilde,
I know that several labs use AG Associates Heatpulse (http://www.ag-rtp.com/). I do believe that MC2 in Gotenburg, Sweden has two. Try asking them about their experiences. We had such a system in our lab more than 15 years ago. It draws a lot of current but is a good little R&D tool.
Jipelec also manufactures table-top RTPs (http://semco-tech.com/jetfirst). We have an older version that is cooled by CDA, so it makes quite a bit of noise. However, nowadays I think they are water cooled.
ATV Technologie GmbH (https://www.atv-tech.com/) manufactures table-top vacuum solder reflow ovens. I have worked with those systems. Nice for R&D and small-scale production.
Best regards,
Leif
Leif S. Johansen
Head of Operations
DTU Danchip
Technical University of Denmark
Danchip
Ørsteds Plads, Byg. 347
2800 Lyngby
Direct +45 45255713
Mobile +45 25348992
lesjo at danchip.dtu.dk
www.danchip.dtu.dk/
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Mathilde Isabelle Barriet
Sent: 29. august 2017 15:17
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Table top RTP oven
Hi
We are looking into purchasing a table top style RTP oven for our cleanroom and I wanted to check if any of you have any brand recommendations for such a system.
Any input will be welcome.
Thanks in advance.
Kind regards,
Mathilde
Senior Engineer
NTNU NanoLab
----------------------------
Sem Sælands vei 14, K1-113
NO-7491 Trondheim
+47 91 89 72 08
www.ntnu.no/nanolab
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
More information about the labnetwork
mailing list