[labnetwork] poly silicon germanium
Robert Vandusen
RobertVandusen at cunet.carleton.ca
Tue Jan 24 17:12:58 EST 2017
Hi everyone.
A client has contacted me looking for polysilicon germanium deposition capability (with germanium less than 20%).
Just wondering if there is anyone on the Labnetwork that might be able to help.
Thanks
Robert Vandusen
Microfabrication and FANSSI Cleanlab Facility Manager
Electronics Department
Carleton University
room: 4184 Mackenzie Building
613-520-2600 ext 5761
rvanduse at doe.carleton.ca<mailto:rvanduse at doe.carleton.ca>