[labnetwork] Ru deposition
DeVito, Richard
rdevito at draper.com
Thu Jul 26 16:18:23 EDT 2018
Nava,
We have e-beam evaporated it for contacts here. There are no toxicity issue I know of..its inert like platinum I believe.
Beware of cracking crucibles on cool down....
RD
Rich DeVito
Principle Member Technical Staff
Group Leader Microfabrication Lab
Draper
555 Technology Square,
Cambridge, MA 02139
Phone: 617-258-3819
www.draper.com<http://www.draper.com/>
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Nava Ariel-Sternberg
Sent: Thursday, July 26, 2018 2:06 PM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Ru deposition
Dear all,
Does anyone have experience with Ru deposition? E-beam or sputtering? Any safety or contamination concerns? Any recommendations?
Thanks,
Nava
Nava Ariel-Sternberg, Ph.D.
Director of CNI Shared Labs
CEPSR/MC 8903
530 west 120th st. NY
NY 10027
Office: 212-8549927
Cell: 201-5627600
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180726/7b1c46da/attachment.html>
More information about the labnetwork
mailing list