[labnetwork] Cleanroom recovery after smoke in intake
Leslie George
leslie.george at ku.ac.ae
Wed Jun 6 03:55:01 EDT 2018
Dear colleagues,
A fire broke out on Monday at one of the retail locations on our campus. The smoke from the fire got into the air intake for our cleanroom, and we can smell smoke throughout the Facility. I'd like to draw on the collective wisdom of the group to help answer the following:
1. Recommend recovery method for the air handling system? (both upstream of the AHU) and downstream including the HEPA's.
2. Recommended cleaning scheme for the interior of the facility?
I appreciate everyone's assistance.
Kind regards,
Leslie George, BSc, MSc
Micro & Nano Fabrication Instructor,
Research Laboratories
Khalifa University - Masdar City Campus
Opposite Presidential Flight Airport
Masdar City, SAF 1A (Undercroft)
Khalifa City A,
United Arab Emirates
P O Box 127788, Abu Dhabi, UAE
T +971 2 810 9227
Fax +971 2 810 9901
M +971 50 84 9720
leslie.george at ku.ac.ae
[cid:image001.png at 01D3DFD3.27E5A010]
ku.ac.ae
[cid:image002.jpg at 01D3E08C.D51AC120]<https://www.facebook.com/khalifauniversity>[cid:image003.jpg at 01D3E08C.D51AC120]<https://www.linkedin.com/school/khalifa-university-/>[cid:image004.jpg at 01D3E08C.D51AC120]<https://twitter.com/KhalifaUni>[cid:image005.jpg at 01D3E08C.D51AC120]<https://www.instagram.com/khalifa_university/>[cid:image006.jpg at 01D3E08C.D51AC120]<https://www.youtube.com/user/KhalifaUniversity>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180606/5e18a53f/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 9620 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180606/5e18a53f/attachment.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image002.jpg
Type: image/jpeg
Size: 973 bytes
Desc: image002.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180606/5e18a53f/attachment.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image003.jpg
Type: image/jpeg
Size: 995 bytes
Desc: image003.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180606/5e18a53f/attachment-0001.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image004.jpg
Type: image/jpeg
Size: 989 bytes
Desc: image004.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180606/5e18a53f/attachment-0002.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image005.jpg
Type: image/jpeg
Size: 997 bytes
Desc: image005.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180606/5e18a53f/attachment-0003.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image006.jpg
Type: image/jpeg
Size: 982 bytes
Desc: image006.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180606/5e18a53f/attachment-0004.jpg>
More information about the labnetwork
mailing list