Hello Mathilde,
Here at LNF (U-Michigan), we have the same problem. We have, also, tried to
buy just the curing agent, but no luck. If you manage to convince Dow to
sell us extra curing agent, please let us know!.
Pilar
On Fri, Mar 2, 2018 at 2:24 AM, Mathilde Isabelle Barriet <
mathilde.i.barriet at ntnu.no> wrote:
> Dear All
> As many of you we are using Sylgard 184. In Norway we have no other choice
> than buying it as a kit (1kg elastomer + 100g of curing agent).
> For some unknown reasons we have many cans of elastomers unused and no
> curing agent to go with... I have been trying to buy the curing agent alone
> through different channels (our supplier, dow corning) but with no success.
> Any of you has any advice or contacts so I can get the curing agent only.
> Thanks
> Kind regards
> Mathilde
>
> Senior Engineer
> NTNU NanoLab
> ----------------------------
> Sem Sælands vei 14, K1-113
> NO-7491 Trondheim
> +47 91 89 72 08
> www.ntnu.no/nanolab
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
--
Pilar Herrera-Fierro, Ph.D.
LNF User Services Director
Lurie Nanofabrication Facility
University of Michigan
RM 1239 EECS Building
1301 Beal Ave.
Ann Arbor, MI 48109-2122
*Cell* 734 646 1399
(734) 646 1399
www.lnf.umich.edu
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180302/06ae3d03/attachment.html>
More information about the labnetwork
mailing list