[labnetwork] Silane and Dichlorosilane Line Evacuation
Morrison, Richard H., Jr
rmorrison at draper.com
Thu Feb 14 08:00:22 EST 2019
Here at Draper the gas is left in the lines at all times, we use double wall stainless and the gas cabinet is tied to the toxic gas monitor. If there is a leak the bottle is automatically shut off. Our gas cabinets are on the floor below the tools so there is a good distance to travel. If we pumped the lines out it would start to get expensive wasting all the gas. The purge of the lines must be done to ensure that there is no exposure to air so vacuum pump down is used and that will take a long time to evacuate the lines, then on the flip side when you repressurize the lines you may run into issues.
You should talk to your university safety group and check the local codes as every jurisdiction has different rules.
Rick
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Bruce Tolleson
Sent: Wednesday, February 13, 2019 1:48 PM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Silane and Dichlorosilane Line Evacuation
Dear users of Silane and Dichlorosilane,
When your systems that use silane and dichlorosilane are not in use do you evacuate the lines going to the tool? We are looking for the best practices for gas line safety in a student environment microelectronic clean room.
The gas lines are wall mount or overhead coaxial stainless steel all welded lines with excess flow sensors.
What are you doing with you silane and dichlorosilane lines?
Thank you,
Bruce E. Tolleson
Rochester Institute of Technology
82 Lomb Memorial Drive, Bldg 17-2627
Rochester, NY 14623-5604
(585) 478-3836
[http://www.rit.edu/~962www/logos/tiger_walking_rit_color.jpg]
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190214/a98cc3cd/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.jpg
Type: image/jpeg
Size: 2550 bytes
Desc: image001.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190214/a98cc3cd/attachment.jpg>
More information about the labnetwork
mailing list