Long,
If you have future plans to do work that is sensitive to magnetic
materials, Fe will completely kill it (eg superconductors). We've
allowed Fe in one evaporator, as some groups need it as catalyst layer
for CNT growth. There was no rust issue. We have yet to allow Fe in
our other evaporators.
Mario
On 2019-02-21 11:39 a.m., Chang, Long wrote:
> Hi All,
>
> I have a user who's wants to sputter Fe in our UHV sputtering system. My director is worried about rust forming. Anyone have adverse experience with Fe I should consider before allowing its usage?
>
> Thanks,
> Long
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
--
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190221/6c99dcdd/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Mario Beaudoin SBQMI sig 2.jpg
Type: image/jpeg
Size: 21446 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190221/6c99dcdd/attachment.jpg>
More information about the labnetwork
mailing list