[labnetwork] Plumbing new gases in ICP-RIE gas pod
Morrison, Richard H., Jr
rmorrison at draper.com
Thu Jan 23 12:04:34 EST 2020
Rick Morrison here from Draper, seems very curious that the CF4 and SF6 lines have a bypass and an input valve. Looks like this is a bypass to maybe vacuum pump the lines during gas bottle hookup or some other function. If that is what those are used for then I would plumb the new gas the same way.
What part of the manifold are you tying the new gases into looks like you have 2 slots open where the SF6 and CF4 lines are.
Rick
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Kevin M McPeak
Sent: Thursday, January 23, 2020 8:42 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Plumbing new gases in ICP-RIE gas pod
Dear Colleagues,
Here at LSU, we want to add C4F8 and CHF3 gases to our Oxford ICP100 system. The gas pod (see attached photo) currently has the following gases plumbed from top to bottom: O2, N2, CF4, and SF6. Notice, the current CF4 and SF6 lines have additional valves and plumbing.
When I add the C4F8 and CHF3 do you recommend I plumb them like the O2 and N2 gases (filter -> MFC -> valve) are or do I need to add the additional valves and plumbing like the SF6 and CF8 lines are? We can do either but the SF6/CF4 method is a lot more money and time. This is an old gas pod, circa 1995 and Oxford has limited information. and advice.
NOTE: The two output lines (top line and 3rd from top) from the gas pod get merged at the tool before entering the instrument. I am not sure why it was plumbed this way back in 1995.
Regards,
Kevin
--
Kevin M. McPeak
Assistant Professor | LSU Dept. of Chemical Engineering
225-578-0058 | mcpeaklab.com | lsu.edu/nanofabrication
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
More information about the labnetwork
mailing list