[labnetwork] laboratory sputter deposition equipment
Soltanian, Saeid
saeid.soltanian at ubc.ca
Fri Jul 17 13:36:42 EDT 2020
I also recommend https://angstromengineering.com/
I have it here and very happy with the performance.
Saeid
--
Saeid Soltanian, PhD
Research Associate, Manager
Centre for Flexible Electronics and Textiles (CFET)
University of British Columbia
117-2355 East Mall, Vancouver, BC V6T 1Z4
Tel: +1-604-827-1573
Email: saeid.soltanian at ubc.ca
http://cfet.ubc.ca/
On Jul 17, 2020, at 8:39 AM, Shimon Eliav <shimonel at savion.huji.ac.il> wrote:
Hi Guido,
I recommend Angstrom Engineering: https://angstromengineering.com/
They are great.
Contact person: Mike Miller (Cc).
Regards,
Shimon
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Guido Janssen - 3ME
Sent: Friday, 17 July 2020 11:30
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] laboratory sputter deposition equipment
Dear colleagues
Here in Delft we are in the proces of replacing our 16 years old AJA sputter tool, used for proces development and materials science studies.
We’re looking for a system with three 2” targets in sputter down configuration able to handle small samples as well as 100 mm wafers. DC and RF, heated substrate holder with sample bias option, turbo pumped and equiped with a load lock.
Do you know of any supplier other than AJA that offers such a system?
Sincerely
Guido Janssen
TU Delft
g.c.a.m.janssen at tudelft.nl
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20200717/8eafff68/attachment.html>
More information about the labnetwork
mailing list