Hello,
I have a user asking about thick film deposition of GdS or GaP in the 5-100 um range.
Does anybody know how people might be doing anything like that?
There seem to be a number of techniques in the sub-micron range.
I'd love to put them in touch with someone that has previous experience.
Thank you.
Jason Tauscher
Manager, Business Outreach and Customer Development
Washington Nanofabrication Facility (WNF)
University of Washington
(206) 616-9409
jbtausch at UW.edu
https://www.wnf.washington.edu/
[cid:image001.png at 01D6C1BD.D208CC60]
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20201124/2c2372dc/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 50475 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20201124/2c2372dc/attachment.png>
More information about the labnetwork
mailing list