Get the SDS of the etchant and see what the etch is made out of.
Then there are on line chemical compatibility charts and see what etches the metals of interest.
Good resource is the CRC Physics and Chemistry handbook and back in the late 1990 there was a paper published by Berkeley that listed etch rates for a tone of semiconductor material, I think the author was Kirt Williams? It was a 2 part article.
Rick
Richard H. Morrison
Principal Member of the Technical Staff
Draper
555 Technology Square
Cambridge, MA
02139-3573
Work 617-258-3420
Cell 508-930-3461
www.draper.com<http://www.draper.com>
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Chong Lee
Sent: Wednesday, February 17, 2021 11:54 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Kanto Chemical BOSE IGZO etchant
I am new to this email list, let me know if this is appropriate to ask:
Does anyone know if above etchant will attack common metals like Al and Mo? Where would I look for data or compatibility chart?
Has anyone used it at MTL before?
Chong
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210217/9491e084/attachment.html>
More information about the labnetwork
mailing list