[labnetwork] Spin Coating VO2 (Vanadyl Acetylacetonate)
Chang, Long
lvchang at Central.UH.EDU
Fri Jan 8 15:15:32 EST 2021
Hello,
A user wants to spin coat VO2 dissolved in methanol. Does anyone know if this is safe to use in a shared spin coater inside a wet bench?