[labnetwork] Looking for PFA or PTFE carriers for thicker wafers
Aaron Hryciw
ahryciw at ualberta.ca
Thu Jan 6 16:55:01 EST 2022
Hi Jeff,
We got a PFA cassette for thick 100 mm wafers last year from Pozzetta
<https://pozzetta.com/>. The part number was CR100A-EMF, and it
accommodated 12 wafers up to 6.28 mm thick. Hope this helps.
Cheers,
– Aaron
Aaron Hryciw, PhD, PEng
Fabrication Group Manager
University of Alberta - nanoFAB
W1-060 ECERF Building
9107 - 116 Street
Edmonton, Alberta
Canada T6G 2V4 Ph: 780-940-7938
www.nanofab.ualberta.ca
On Thu, Jan 6, 2022 at 2:46 PM Salzmann, Jeffrey <
Jeffrey.Salzmann at integer.net> wrote:
> Hello!
>
> I am working with 100mm wafers, but they’re up to 2mm thick (versus the
> standard 525/625µm).
>
>
>
> Does anyone have a recommendation or contact I could use to procure these?
>
>
>
> Thanks!
> Jeff
>
>
>
> *Jeff Salzmann*
>
> Senior Research Engineer
>
> Advanced Materials Technology Group
>
>
>
> *Integer* *
>
> 10000 Wehrle Drive
>
> Clarence, NY, 14031
>
> Tel +1 716.759.5796
>
> Cell +1 716.867.1302
>
> Jeffrey.Salzmann at integer.net
>
> www.integer.net
>
>
>
> ** Integer comprises the following companies: *
>
> Greatbatch Medical -‐ Lake Region Medical -‐ Electrochem
>
>
>
> ------------------------------
>
> Integer Confidentiality Notice: This electronic mail transmission is
> intended for the use of the individual or entity to which it is addressed
> and may contain confidential or proprietary information belonging to the
> sender. If you are not the intended recipient, you are hereby notified that
> any disclosure, copying, distribution, or the taking of any action in
> reliance on the contents of this information is strictly prohibited. If you
> have received this transmission in error, please notify the sender
> immediately by e-mail and delete the original message. Thank you for your
> cooperation.
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220106/b243e9c6/attachment.html>
More information about the labnetwork
mailing list